Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East) GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL3000 PC Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 50.0 - 130 °C | 122 - 266 °F | Average value: 92.0 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific) Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
UL RTI, Mechanical without Impact | 50.0 - 60.0 °C | 122 - 140 °F | Average value: 52.7 °C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
UL RTI, Mechanical without Impact | 50.0 - 90.0 °C | 122 - 194 °F | Average value: 78.3 °C Grade Count:26 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.700 - 3.00 mm |
122 °F @Thickness 0.0276 - 0.118 in |
|
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl HF180 PPE+HIPS (Europe-Africa-Middle East) NORYL HF180 is an unfilled, flame retardant material with a Vicat B/120 of 100°C according ISO 306. NORYL HF180 is V1 at 2.0 mm according UL94 and halogenThis data was supplied by SABIC-IP for th.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1543 PPE+PS |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1543 PPE+PS (Asia Pacific) |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 6500-70 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded .. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |