Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR15 ABS
Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific)
Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38F ABS
Very high impact ABS. Toughness/rigidity. FDA compliant.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. FDA compliant.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38N ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)>
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MGABS01 ABS
Injection molding ABS. High impact, high gloss, good flow.
CTE, linear, Transverse to Flow 86.4 - 130 µm/m-°C
48.0 - 72.2 µin/in-°F
Average value: 101 µm/m-°C Grade Count:25
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 3706 PBT+PC
Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors.
CTE, linear, Transverse to Flow 86.4 µm/m-°C

@Temperature -40.0 - 37.8 °C
48.0 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed..
Copyright © lookpolymers.com All Rights Reserved