Mechanical Properties Metric English Comments
Charpy Impact, Notched >= 0.110 J/cm²
>= 0.524 ft-lb/in²
ISO 179
Perstorp Compounds 171 Urea-Formaldehyde w/ cellulose filler
Information provided by Perstorp Compounds Inc.
Charpy Impact, Notched >= 0.110 J/cm²
>= 0.524 ft-lb/in²
1eU; ISO 179
Perstorp Compounds AMITEC 751 Melamine
Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.Information provided by Perstorp Compounds Inc.
Charpy Impact, Notched 0.110 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
0.524 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.507 J/cm² Grade Count:20
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Charpy Impact, Notched 0.110 J/cm²

@Temperature 23.0 °C
0.524 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® B3S25 PA6 Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 0.110 J/cm²

@Temperature 23.0 °C
0.524 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 179/1eA
SYNTHOS Krasten® 662E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa..
Charpy Impact, Notched 0.110 J/cm² - NB
0.524 ft-lb/in² - NB
Average value: 2.47 J/cm² Grade Count:211
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.110 J/cm²

@Temperature -30.0 °C
0.524 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Centrex® HGM ASA Blend  (discontinued **)