Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 - 1.16 g/cc @Temperature 200 - 215 °C |
0.0412 - 0.0419 lb/in³ @Temperature 392 - 419 °F |
Average value: 1.15 g/cc Grade Count:6 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 1.05 - 1.16 g/cc | 0.0379 - 0.0419 lb/in³ | Average value: 1.09 g/cc Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Density | 1.00 - 1.16 g/cc | 0.0361 - 0.0419 lb/in³ | Average value: 1.08 g/cc Grade Count:128 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Density | 1.04 - 1.16 g/cc | 0.0376 - 0.0419 lb/in³ | Apparent |
Gouda Vuurvast FI 55-11 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.10 - 1.16 g/cc | 0.0397 - 0.0419 lb/in³ | 262B Resin |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Density | 1.15 - 1.16 g/cc | 0.0415 - 0.0419 lb/in³ | |
Solvay MACKSTAT® DM Surfactant Product Description: Mackstat DM is a 55% active solution of DMDM Hydantoin, a very effective broad spectrum antimicrobial for cosmetic and personal care products. Due to its high water solubility, .. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of.. |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 60/R1 Flexible PVC, Injection Molding for Footwear Anti-accident soles |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 45/K Medical Flexible PVC, Extrusion Tubular apparatus |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 270A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 470A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.12 - 1.16 g/cc | 0.0405 - 0.0419 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |