Thermal Properties Metric English Comments
Glow Wire Test 750 °C
1380 °F
Plastcom SLOVALEN PC 51 C 20 PP, 20% mineral filling
FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C..
Glow Wire Test 750 °C
1380 °F
STN IEC 60695-2-10
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C...
Glow Wire Test 750 °C
1380 °F
STN IEC 60695-2-10
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Glow Wire Test 750 °C
1380 °F
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre
Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi..
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific)
CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PP CQX10030 RT Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific)
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPHC K2040H Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 3.20 mm
1380 °F

@Thickness 0.126 in
IEC 60695-2-12
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East)
GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PP HIP8040 VT2 Polypropylene, Mineral Reinforced, Heat Resistant
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPH T5020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP
BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne..
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP
BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of ..
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP
SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f..
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Europe-Africa-Middle East)
Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements..
Glow Wire Test 750 °C
1380 °F
60695-2-10
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Glow Wire Test 750 °C
1380 °F
Polyram RamSter PF300J50 PBT, 50% Glass Fiber + Glass beads
50% Glass-fiber and glass beads reinforced PBT.Information provided by Polyram Ram On Ind.
Glow Wire Test 750 °C
1380 °F
I.E.C. 695-2-12
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend
Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Glow Wire Test <= 750 °C

@Thickness 3.00 mm
<= 1380 °F

@Thickness 0.118 in
IEC 695
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPH TS8030 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Glow Wire Test 750 °C

@Thickness 3.20 mm
1380 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Copyright © lookpolymers.com All Rights Reserved