Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.45 - 2.07 GPa | 210 - 300 ksi | Average value: 1.69 GPa Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Modulus of Elasticity | 1.45 - 2.85 GPa | 210 - 413 ksi | Average value: 2.28 GPa Grade Count:59 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Modulus of Elasticity | 1.45 GPa | 210 ksi | ASTM D638 |
Total PPH 3825 Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio.. |