Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 0.110 J/cm² | >= 0.524 ft-lb/in² | ISO 179 |
Perstorp Compounds 171 Urea-Formaldehyde w/ cellulose filler Information provided by Perstorp Compounds Inc. |
|||
Charpy Impact, Notched | >= 0.110 J/cm² | >= 0.524 ft-lb/in² | 1eU; ISO 179 |
Perstorp Compounds AMITEC 751 Melamine Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.Information provided by Perstorp Compounds Inc. |
|||
Charpy Impact, Notched | 0.110 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
0.524 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.507 J/cm² Grade Count:20 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Charpy Impact, Notched | 0.110 J/cm² @Temperature 23.0 °C |
0.524 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B3S25 PA6 Unreinforced Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 0.110 J/cm² @Temperature 23.0 °C |
0.524 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Charpy Impact, Notched | 0.110 J/cm² - NB | 0.524 ft-lb/in² - NB | Average value: 2.47 J/cm² Grade Count:211 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.110 J/cm² @Temperature -30.0 °C |
0.524 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |