Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 40.7 - 115 MPa | 5900 - 16600 psi | Average value: 69.4 MPa Grade Count:77 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Flexural Yield Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9025 , 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 40.7 MPa @Thickness 6.40 mm |
5900 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Flexural Yield Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Yield Strength | 40.7 - 240 MPa | 5900 - 34800 psi | Average value: 112 MPa Grade Count:28 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Flexural Yield Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Samyang Trilen® 9550T30 Polypropylene, Reinforced Mechanical strength and thermal resistance are excellent.9550T30 is a non-flame retardant, reinforced grade.Information provided by Samyang. |