Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL3000 PC Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | Average value: 50.0 °C Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
UL RTI, Mechanical without Impact | 50.0 - 115 °C | 122 - 239 °F | Average value: 66.0 °C Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific) Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.700 - 3.00 mm |
122 °F @Thickness 0.0276 - 0.118 in |
|
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet
(discontinued **) Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.950 - 2.90 mm |
122 °F @Thickness 0.0374 - 0.114 in |
|
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+PS LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 7500-80 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1391 PPE+PS PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 50.0 - 80.0 °C | 122 - 176 °F | Average value: 56.0 °C Grade Count:5 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |