LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
Latamid
|
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced |
Nylon 66, 20% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced |
Nylon 66, 30% Carbon Fiber Filled |
Latamid
|
LATI Latamid 66 E21 PA 66, Impact Modified |
Nylon 66, Impact Grade |
Latamid
|
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 40% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 40% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 40% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 50% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 50% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 50% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 50% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 60% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized |
Nylon 66, 30% Carbon Fiber Filled |
Latamid
|
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized |
Nylon 66, 40% Carbon Fiber Filled |
Latamid
|
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized |
Nylon 66, 50% Carbon Fiber Filled |
Latamid
|
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced |
Nylon 66, 10% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
Latamid
|
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
Latamid
|
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, Heat Stabilized |
Latamid
|
LATI Latamid 66 MDT03-01 PA 66 |
Nylon 66 |
Latamid
|
LATI Latamid 66 MDT05-01 PA 66 |
Nylon 66 |
Latamid
|
LATI Latamid 66 PA 66 |
Nylon 66, Unreinforced |
Latamid
|
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 30% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, 40% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
Latamid
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced |
Nylon 66, Glass Bead Filled |
Latamid
|
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 30% Glass Fiber Filled |
Latamid
|
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 50% Glass Fiber Filled |
Latigloss
|
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 60% Glass Fiber Filled |
Latigloss
|
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized |
Nylon 66, 30% Carbon Fiber Filled |
Latigloss
|
LATI Latigray 66-01 CX/50 PA 66 |
Nylon 66, Unreinforced |
Latigray
|
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced |
Nylon 66, Aramid Fiber Filled |
Latilub
|
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled |
Nylon 66, Glass Fiber/MoS2 Filled |
Latilub
|
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled |
Nylon 66, Glass Fiber/MoS2 Filled |
Latilub
|
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled |
Nylon 66, Glass Fiber/MoS2 Filled |
Latilub
|
LATI Latilub 66-02S PA66, Silicone Filled |
Nylon 66 |
Latilub
|
LATI Latilub 66-10T G/10 PA66, 10% Glass Fiber Reinforced, PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled |
Nylon 66, Carbon Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-10T Y/15 PA66, 15% Aramid Fiber Reinforced, PTFE Filled |
Nylon 66, Aramid Fiber Filled |
Latilub
|
LATI Latilub 66-15T G/30 PA66, 30% Glass Fiber Reinforced, PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-15T K/30 PA66, 30% Carbon Fiber Reinforced, PTFE Filled |
Nylon 66, Carbon Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled |
Nylon 66, PTFE Filled |
Latilub
|
LATI Latilub 66-20T G/20 PA66, 20% Glass Fiber Reinforced, PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 66-20T PA66, PTFE Filled |
Nylon 66, PTFE Filled |
Latilub
|
LATI Latimass 63-06 D025 PA66 |
Nylon 66, Unreinforced |
Latimass
|
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced |
Nylon 66, 20% Glass Fiber Filled |
Latiohm
|
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced |
Nylon 66, 20% Glass Fiber Filled |
Latiohm
|
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Latiohm
|
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced |
Nylon 66, 40% Glass Fiber Filled |
Latiohm
|
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant |
Nylon 66, 30% Glass Fiber Filled |
Latishield
|
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced |
Nylon 66, Stainless Steel Filled; EMI Grade |
Latishield
|
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized |
Nylon 66, Stainless Steel Filled; EMI Grade |
Latishield
|
LATI Latishield 66-10A PA66, Steel Fiber Reinforced |
Nylon 66, Stainless Steel Filled; EMI Grade |
Latishield
|
LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced |
Nylon 66, Stainless Steel Filled; EMI Grade |
Latishield
|
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Latistat
|
LATI Latistat 66-06 PA66 |
Nylon 66, Unreinforced |
Latistat
|
LATI Latistat 67-08 PA66, Impact Modified |
Nylon 66, Impact Grade |
Latistat
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Kelon® A
|
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 40% Glass Fiber Filled |
Latamid
|
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized |
Nylon 66, 20% Carbon Fiber Filled |
Latamid
|
LATI Latilub 66-01M PA66, Molybdenum disulphide Filled |
Nylon 66, MoS2 Filled |
Latilub
|
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latiohm
|
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized |
Nylon 66, 10% Mineral Filled |
Latiohm
|
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 40% Glass Fiber Filled |
Latiohm
|
LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized |
Nylon 66, 40% Mineral Filled |
Kelon® A
|
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized |
Nylon 66, Glass/Mineral Filled |
Kelon® A
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Latamid
|
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|
LATI Latilub 67-10STE21 G/20 PA66, 20% Glass Fiber Reinforced, Silicone/PTFE Filled |
Nylon 66, Glass Fiber/PTFE Filled |
Latilub
|