LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Stainless Steel Filled; EMI Grade
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
Linear Mold Shrinkage, Flow 0.0045 - 0.0075 cm/cm
0.0045 - 0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 5.90 GPa
856 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
Vicat Softening Point 245 °C

@Load 5.00 kg
473 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 200 ohm-cm
200 ohm-cm
Surface Resistance 20 ohm
20 ohm
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 90.0 - 100 °C
194 - 212 °F
Descriptive Properties Value Comments
Electromagnetic reflection 93 dB
ISO Shrinkage - Pressure 60 MPa