Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Premix Thermoplastics Inc.
Trade Name PRE-ELEC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has been developed for extrusion of thermoformable multilayer sheets and injection molding. It has been designed to full strict ionic purity requirements. Surface resistance values of 108 O (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters. The products made out of PRE-ELEC® ESD 6610 are washable, reusable, recyclable. PRE-ELEC® ESD 6610 is whitish in colour and can be coloured into various bright colours.Applications: Injection moulded boxes, bins, thermoformed trays and clamshells when permanent ESD protection is required. These products can be used in electronics, medical, pharmaceutical and paper handling industries.Processing: PRE-ELEC® ESD 6610 compound can be processed in normal processing conditions as with polystyrene.Test Specimen: 10[mm] wide moulded rodInformation from Premix OY
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Thickness 102 microns
4.00 mil
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ISO 294-4
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70

@Thickness 1.00 mm
70

@Thickness 0.0394 in
ISO 868
Tensile Strength 16.0 MPa
2320 psi
ISO 527
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
1.90 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO) 14.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
6.66 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
75/Method Bf
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
75/Method Af
Vicat Softening Point 84.0 °C
183 °F
ISO 306/B50
98.0 °C
208 °F
ISO 306/A50
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 ohm

@Thickness 0.00100 mm
1.00e+9 ohm

@Thickness 0.0000394 in
ISO IEC 61340-5-1
Static Decay <= 1.0 sec

@Thickness 1.00 mm
<= 1.0 sec

@Thickness 0.0394 in
ISO IEC 61340-5-1
Processing Properties Metric English Comments
Zone 1 180 °C
356 °F
Cylinder
200 °C
392 °F
Die
Zone 2 190 °C
374 °F
Cylinder
200 °C
392 °F
Die
Zone 3 190 °C
374 °F
Die
200 °C
392 °F
Cylinder
Zone 4 200 °C
392 °F
Die
200 °C
392 °F
Cylinder
Zone 5 200 °C
392 °F
Die
200 °C
392 °F
Cylinder
Melt Temperature 190 - 210 °C
374 - 410 °F
Mold Temperature 30.0 - 70.0 °C
86.0 - 158 °F
Roll Temperature 50.0 °C
122 °F
3rd Roll
60.0 °C
140 °F
1st Roll
60.0 °C
140 °F
2nd Roll
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Pre-drying in a dehumidifier
Dry Time 3 - 4 hour
3 - 4 hour
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Hold Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Post Pressure
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Injection Speed Moderate