Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 200 °C | 392 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 4 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 4 | 200 °C | 392 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b.. |
|||
Zone 4 | 200 °C | 392 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Zone 4 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Zone 4 | 200 °C | 392 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded.. |
|||
Zone 4 | 200 - 220 °C | 392 - 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as.. |
|||
Zone 4 | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r.. |
|||
Zone 4 | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 4 | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 4 | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® R195A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 4 | 200 - 210 °C | 392 - 410 °F | Injection |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Zone 4 | 200 °C | 392 °F | Nozzle |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Zone 4 | 200 °C | 392 °F | Nozzle |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Zone 4 | 200 °C | 392 °F | Nozzle |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Zone 4 | 200 °C | 392 °F | Nozzle |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Zone 4 | 200 °C | 392 °F | Nozzle |
BASF Ultraform® N2520 XL2 POM Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF |