Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Zone 1 | 180 °C | 356 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Zone 1 | 180 °C | 356 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Blow Molding |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | Extrusion Molding |
LG Chemical SH610S ABS, Excellent Surface, High Impact Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 180 - 210 °C | 356 - 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Zone 1 | 180 - 195 °C | 356 - 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Zone 1 | 180 °C | 356 °F | |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 1 | 180 °C | 356 °F | |
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 1 | 180 °C | 356 °F | Barrel Temp of Main Extruder |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Star L POM D61 POM, Injection Molded Star L POM D61 is a PTFE/Silicone Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Star L POM D84 POM, Injection Molded Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam MF0044 PP, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam MF0044 is a Halogen Free Flame Retardant, Glass Fiber Reinforced, PP Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® LGC90-QX POM, 26% Glass Reinforced Preliminary Data Sheet26% long fiber glass filled, high strengthLong Fiber Reinforced Thermoplastic products may be processed using current standard injection molding machines having screw diameters.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 °C | 356 °F | Extrusion |
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® CP15X POM
(Unverified Data**) Preliminary Data Sheetcreep resistant, high viscosity acetal copolymerInformation provided by Celanese |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |