Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 15 FRG 2 LW PA6, 15% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 960°.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 20 FRG 3 PA6, 20% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 20 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 9.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 T 10 PA6, mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Mold Temperature | 30.0 - 70.0 °C | 86.0 - 158 °F | |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Mold Temperature | 16.0 - 70.0 °C | 60.8 - 158 °F | Average value: 36.2 °C Grade Count:51 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | Injection |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Start Point: 60°C |
Kingfa PA66-RG001 Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation Provided by Kingf.. |
|||
Mold Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Mold Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Mold Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Chi Mei Acryrex® CM-205 PMMA High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather .. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan 685 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan C 88 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Mold Temperature | 20.0 - 70.0 °C | 68.0 - 158 °F | |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Ejection temperature |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Asahi Kasei Xyron® 240V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection molding |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Mold Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |