Processing Properties Metric English Comments
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPC T20020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH T16040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 150 °C
158 - 302 °F
Average value: 98.7 °C Grade Count:15
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH K5040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH T15020 H4 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 °C
158 °F
For 2 hours or vented barrel
Polimeri Europa Edistir RKL Polystyrene  (discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App..
Drying Temperature 70.0 - 88.0 °C
158 - 190 °F
Average value: 77.4 °C Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Drying Temperature 70.0 - 100 °C
158 - 212 °F
Average value: 85.4 °C Grade Count:15
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Drying Temperature 70.0 - 121 °C
158 - 250 °F
Average value: 88.5 °C Grade Count:15
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Extrusion Molding
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
LG Chemical LUPOL GP3202Z PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Drying Temperature 70.0 - 90.0 °C
158 - 194 °F
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Drying Temperature 70.0 - 100 °C
158 - 212 °F
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Extrusion Molding
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
LG Chemical LUPOL HM5302W PP+MF30%, High Impact
Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Drying Temperature 70.0 - 90.0 °C

@Time 10800 sec
158 - 194 °F

@Time 3.00 hour
LATI Laticonther 83 CP/85 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Lubrizol Estane® S392A Thermoplastic Polyurethane
Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow ..
Drying Temperature 70.0 °C
158 °F
Pre drying temperature
Total PSI 4440(AS) High Impact Polystyrene
4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, ..
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding
Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 70.0 °C

@Time 14400 sec
158 °F

@Time 4.00 hour
Eurostar Starpylen HU 70E4 ECR
Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar.
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding
Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Celanese Celstran® PA66-GF50-02-US Nylon 66, 50% Glass Reinforced
50 % Long glass fiber reinforced, heat stabilized, Nylon 6/6Information provided by Celanese
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature 70.0 - 80.0 °C

@Time 10800 sec
158 - 176 °F

@Time 3.00 hour
LATI Latilub 30/R-07GRT PC, Graphite/PTFE Reinforced
Self-lubricating product based on Polystyrene (PS). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo..
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Polykemi AB POLYfill PPH TS2040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Drying Temperature <= 70.0 °C
<= 158 °F
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Drying Temperature 70.0 - 90.0 °C
158 - 194 °F
Average value: 78.4 °C Grade Count:13