Hold Pressure |
40.0 - 90.0 MPa |
5800 - 13100 psi |
|
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended.. |
Hold Pressure |
40.0 - 90.0 MPa |
5800 - 13100 psi |
|
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Information provided by PolyOne |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP10 GR50 NL PPCP, 50% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® HP30 NL XC30 PPHP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural
Information provided by Eurotec® |
Hold Pressure |
40.0 - 80.0 MPa |
5800 - 11600 psi |
|
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |