A. Schulman POLYBLAK™ 3225 Superior Black Color Concentrate, 50% Carbon Black Based In PP Homopolymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 3225 Superior Black Color Concentrate, 50% Carbon Black Based In PP Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBLAK® Black 3225 is a superior black color concentrate containing 50% carbon black in PP homopolymer. This masterbatch is designed to provide uniform opacity and a regular blue undertone with pigment particle size of 75 nanometers. POLYBLAK® Black 3225 is formulated for general use in polypropylene injection molding applications. POLYBLAK® Black 3225 is typically recommended for use at 5% addition levels.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Carbon Black Loading 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789