Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injecti.. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti.. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
Huntsman PE1651 EVA Film Extrusion
(discontinued **) 6.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with outstanding low temperature strength, excellent clarity, and good heat seal.Applications: Film extrusion: ice bags, liqui.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/hr; 50N |
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade
(discontinued **) OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :.. |
|||
Vicat Softening Point | 84.0 - 118 °C | 183 - 244 °F | Average value: 99.9 °C Grade Count:29 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
LyondellBasell Petrothene® NA206000 Low Density Polyethylene ApplicationsPETROTHENE NA 206-000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a 3 lb/ream coating weight at lin.. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
Vicat Softening Point | 84.0 - 86.0 °C @Load 5.00 kg |
183 - 187 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 321 Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Vicat Softening Point | 84.0 °C | 183 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL V081 PPE+HIPS (Europe-Africa-Middle East) NORYL V081 is a high flow, UV stabilized PPO/PS blend for TV backplate applications. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 175A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ASTM D1525 |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1020 VB 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.ISO data provided by the manufacturer, Arke.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
BASF Polystyrol® 454 C Impact Grade Polystyrene (Europe) Easy flowing, medium-impact grade.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 84.0 - 128 °C | 183 - 262 °F | Average value: 91.9 °C Grade Count:44 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin