Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH GF5010 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH T4060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | 48 hours max. |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | No venting in an air circulating oven |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | nominal; maximum drying time of 8 hours |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Dry Time | 2 - 4 hour @Temperature 79.4 °C |
2 - 4 hour @Temperature 175 °F |
to ensure moisture content is less than 0.2% |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 71.1 °C |
2 - 4 hour @Temperature 160 °F |
to eliminate surface defects |
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 121 °C |
2 - 4 hour @Temperature 250 °F |
to ensure moisture level is less than 0.2% |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 104 °C |
2 - 4 hour @Temperature 220 °F |
to ensure moisture level is less than 0.02% |
Clariant Renol PUR1100SS15 Polyurethane Elastomer, Stainless Fiber, EMI/RFI/ESD Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Diamond Polymers ABS 1100 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |