Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 40.0 - 60.0 MPa | 5800 - 8700 psi | Post Pressure |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Hold Pressure | 40.0 - 60.0 MPa | 5800 - 8700 psi | Post Pressure |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis BF335SA Polypropylene Copolymer BF335SA is a polypropylene copolymer intended for injection molding. This material has a very high impact strength while maintaining good stiffness, gives a good surface quality and is
easy to proc.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Xmod™ GB306SAF Polypropylene, Glass Fiber Reinforced Xmod™ GB306SAF is a 35 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. The product is available in standard black 9502. This mat.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF209AE Polypropylene TPO Compound Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |