Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, L OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, Q OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, SL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 190-1323 LMDPE Rotational Molding Resin Description: ICORENE 190-1323 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic ole.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ XFBR712 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ XFBR712 medium melt flow, 1,800 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact resistance.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM-D638 |
Polyram RamOfin PL108 LUBRICATED COMPUND FOR PIPES DUCTING, Lubricated Lubricated polyethylene specially developed for optical fiber communication pipesInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior .. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ BNT 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South A.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min |
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided .. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437M10L Mica Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W10L Wollastonite Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W30L1 Wollastonite Reinforced |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ASTM D638/ISO 527 |
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene Description: UTEC3040 is an Ultra High Molecular Weight Polyethylene with a molecular weight about 10 times higher than High Density Polyethylene (HDPE) resins. This extremely high molecular weight .. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers DEXFLEX® 930HS TPO
(discontinued **) Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a.. |