Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S KA 40A-3S1767 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
PolyOne OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5400 series are based upon alloys of SEBS and aliphatic TPU, combining the adv.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 74.3 °C Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa FRHIPS-980 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold.. |
|||
Mold Temperature | 30.0 - 100 °C | 86.0 - 212 °F | suitable temperature 40-60°C |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Mold Temperature | 30.0 - 100 °C | 86.0 - 212 °F | suitable temperature 40-60°C |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
Borealis Daplen™ ED206HP TPO Compound Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scra.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ AK4504 TPO Compound Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low th.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Mold Temperature | 30.0 - 65.6 °C | 86.0 - 150 °F | |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 30.0 - 90.0 °C | 86.0 - 194 °F | |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Mold Temperature | 30.0 - 40.0 °C | 86.0 - 104 °F | |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |