Processing Properties Metric English Comments
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 7100
PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® PS 1328
PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Panipol Oy DXH-PP Inherently Conductive Polymer
Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr..
Injection Pressure 75.2 - 120 MPa
10900 - 17400 psi
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Injection Pressure >= 75.2 MPa
>= 10900 psi
Panipol Oy DXH Inherently Conductive Polymer
Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade..