Polymer Property : Dry Time = 4 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 2 - 4 hour
2 - 4 hour
in fresh-air dryer
Polykemi AB POLYabs S00 ABS, High Flow
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in fresh-air dryer
Polykemi AB POLYasa 3010F Extra High Flow ASA
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
Polykemi AB POLYfill PPC K20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in desiccant air dryer
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
Polykemi AB POLYfill PPH T15040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
PTS PCA-3013 High Flow PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Dry Time 2 - 4 hour
2 - 4 hour
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (DAM)
Information provided by Ravago.
Dry Time 2 - 4 hour
2 - 4 hour
in fresh-air dryer
Polykemi AB POLYabs F20 ABS
Information provided by Polykemi AB
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
Polykemi AB POLYfill PPH GF5040 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Dry Time 3 - 4 hour
3 - 4 hour
48 hours max.
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Dry Time 3 - 4 hour
3 - 4 hour
nominal; maximum drying time of 8 hours
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc.
Dry Time 2 - 4 hour
2 - 4 hour
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
Dry Time 2 - 4 hour
2 - 4 hour
Option 3
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Dry Time 2 - 4 hour
2 - 4 hour
Option 3
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Dry Time 2 - 4 hour
2 - 4 hour
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene
Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH.
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66
Information provided by A. Schulman.
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Dry Time 1 - 4 hour
1 - 4 hour
Hydraulic Set Time, Initial
Zircar Ceramics ZIRALCAST 95 Alumina Refractory Castable
Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applica..
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
A. Schulman ComAlloy® E-12672 Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Dry Time 2 - 4 hour

@Temperature 79.4 °C
2 - 4 hour

@Temperature 175 °F
to ensure moisture content is less than 0.2%
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Dry Time 2 - 4 hour

@Temperature 79.4 °C
2 - 4 hour

@Temperature 175 °F
to ensure moisture content is less than 0.2%
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches
Dry Time 2 - 4 hour

@Temperature 85.0 °C
2 - 4 hour

@Temperature 185 °F
to ensure moisture content is less than 0.05%
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant
Data provided by Clariant Masterbatches
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture level is less than 0.02%
Clariant Renol TPU2087AFR Polyurethane Elastomer, Flame Retardant
Data provided by Clariant Masterbatches
Dry Time 2 - 4 hour
2 - 4 hour
Diamond Polymers ABS VP-11
Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Dry Time 2 - 4 hour
2 - 4 hour
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Dry Time 2 - 4 hour
2 - 4 hour
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Dry Time 2 - 4 hour
2 - 4 hour
BASF Nypel® 2314 HS BK6 PA6 (Dry)
Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: go..