Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 190 - 230 °C
374 - 446 °F
Polykemi AB POLYabs N30 ABS
Information provided by Polykemi AB
Melt Temperature 190 - 230 °C
374 - 446 °F
Polykemi AB POLYabs P0P ABS, Plating Grade
Information provided by Polykemi AB
Melt Temperature 190 - 230 °C
374 - 446 °F
Polykemi AB POLYabs SS0 ABS, High Flow
Information provided by Polykemi AB
Melt Temperature 190 - 210 °C
374 - 410 °F
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
Melt Temperature 190 - 210 °C
374 - 410 °F
SABIC BM6246LS High Density Polyethylene for Blow Molding
Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes..
Melt Temperature 190 - 274 °C
374 - 525 °F
Ineos Nova FX510 Super High Impact Polystyrene  (discontinued **)
Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi..
Melt Temperature 190 - 274 °C
374 - 525 °F
Ineos Nova 1531 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p..
Melt Temperature 190 - 274 °C
374 - 525 °F
Ineos Nova 4214 Medium Impact Polystyrene  (discontinued **)
Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o..
Melt Temperature 190 - 230 °C
374 - 446 °F
Celanese Hostaform® C 27021 AS POM, Specialty  (Unverified Data**)
POM copolymerAntistatic grade, easy flowInformation provided by Celanese
Melt Temperature 190 - 205 °C
374 - 401 °F
Injection
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester
Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par..
Melt Temperature 190 - 220 °C
374 - 428 °F
Injection Molding
LG Chemical ALPHALAC SG960 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical
Melt Temperature 190 - 200 °C
374 - 392 °F
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Melt Temperature 190 - 210 °C
374 - 410 °F
Extrusion
Stellarchem LP-830 TPE Compound
This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
Melt Temperature 190 - 205 °C
374 - 401 °F
Extrusion
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-1011A Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Temperature 190 - 210 °C
374 - 410 °F
Covestro Desmopan® DP 2786A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Melt Temperature 190 - 220 °C
374 - 428 °F
Covestro Desmopan® DP 2792A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Melt Temperature 190 - 200 °C
374 - 392 °F
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding
Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 190 - 240 °C
374 - 464 °F
Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding
Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 190 - 230 °C
374 - 446 °F
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection-molding
BASF Ultraform® N2200 G43 POM
Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection molding
BASF Ultraform® S2320 003 POM
Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF
Melt Temperature 190 - 230 °C
374 - 446 °F
Injection-molding
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Melt Temperature 190 - 210 °C
374 - 410 °F
Celanese Hostaform® C 13031 LS POM, UV Resistant
POM copolymerInformation provided by Celanese
Melt Temperature 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 27064 XAP2® POM, Impact Modified
Description: Easy flowing, elastomer-containing injection molding type based on HOSTAFORM C 27021 with high toughness and reduced emissionsHB. Burning rate ISO 3795 and FMVSS 302 < 100 mm/min for mo..
Melt Temperature 190 °C
374 °F
Chem Polymer Formax 604 Acetal, Low Flow
A 4 melt flow index copolymer acetal for extrusion or thick injection molding applications.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 190 °C
374 °F
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced
A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 190 - 200 °C
374 - 392 °F
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic  (Unverified Data**)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
Melt Temperature 190 - 274 °C
374 - 525 °F
Ineos Nova 6110 Super High Impact Polystyrene  (discontinued **)
Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen..