Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | <= 1.20 GPa | <= 174 ksi | |
Reliance Industries Polypropylene - Virgin Polypropylene Information provided by Reliance Industries |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP FARADEX MX10014 PP (Europe-Africa-Middle East) LNP* Faradex* Mx10014 is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Flexural Modulus | 1.20 - 7.20 GPa @Temperature -40.0 - 80.0 °C |
174 - 1040 ksi @Temperature -40.0 - 176 °F |
Average value: 4.55 GPa Grade Count:1 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer Primary Processing Method: Injection MoldingKey Features: good cold impact resistance, good stiffness and impact balance, excellent dimensional stability, FDA acceptableApplications: seating, applia.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant Primary Processing Method: Injection MoldingKey Features: resistant to aging at high temperatures in both wet and dry environments, good cold impact resistance, excellent dimensional stability, FDA .. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityAppli.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, Conditioned Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Borealis Borcoat™ BB108E-1199 White Polypropylene Block Copolymer for Steel Pipe Coating Borcoat BB108E-1199, a ready made white compound, is a highly molecular weight, low melt flow polypropylene block copolymer. As a top-coat in three component polypropylene systems, Borcoat BB108E-1.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 29 H HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Total PPR 7227 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 7227 is a high transparency random copolymer polypropylene specially developed for the injection molding of caps and closures and articles with high transparency, excellent .. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Wet; ASTM D790 |
Asahi Kasei Leona® 1700S Nylon 66 Similar to 1500 but with even higher molecular weight. Suitable for extrusion of thick-wall parts.Applications:Rods, films Information provided by Asahi Kasei |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |