Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, DG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, SL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D412 |
Precision Polymer Engineering E85Q Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Fo.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 500 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-1/1A/50 |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, CL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, W OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-1, -2 |
LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic ole.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | |
Sibur MPP 23007-E10 Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Tensile Strength, Yield | 17.0 MPa | 2460 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098C-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific) LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationExcellent impac.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ BNT 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific,.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ASTM D638/ISO 527 |
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene Description: UTEC3040 is an Ultra High Molecular Weight Polyethylene with a molecular weight about 10 times higher than High Density Polyethylene (HDPE) resins. This extremely high molecular weight .. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ASTM D638/ISO 527 |
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D-638 |
Bapolene® 3042U Polyethylene, Rotational Molding Grade Bapolene 3042U is a hexene linear low density polyethylene designed to provide an excellent combination of ESCR and impact. It contains a UV additive package and complies with US FDA 21CFR177.1520... |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | |
BASF Procom® D 1173 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D368 |
Reliance Industries Reclair Crosslinked R35042 Crosslinkable R35042 is a polyethylene grade that has increased service temperature and toughness, and improved ESCR over Reclair R35042. Crosslinkable R35042 applications include fuel tanks and ch.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers DEXFLEX® 826HS TPO
(discontinued **) Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and.. |