Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PH 69 GF 30 TSM PP, 30% glass fibre, mod. of mech. prop., thermal stability FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Thermo stable. Increased strength in comparison wi.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PH 69 GF 40 TS PP reinforced with 40% glass fibre, with modification of mechanical properties and thermal stabilization Features: Modified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled P.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PQ 81 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 10 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b.. |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Injection Pressure | 80.0 - 120 MPa | 11600 - 17400 psi | |
Beijing Chemical Industry KAIFA® 301-G15F PBT Resin 15% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
Plastcom SLOVALEN PH 81 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Injection Pressure | 80.0 - 120 MPa | 11600 - 17400 psi | |
Zhejiang Juner PC-A1-9A Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 50.0 - 120 MPa | 7250 - 17400 psi | |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |