Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.20 GPa | 174 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Flexural Modulus | 1.20 - 1.50 GPa | 174 - 218 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Modulus | >= 1.20 GPa | >= 174 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact.. |
|||
Flexural Modulus | 1.20 - 7.20 GPa @Temperature -40.0 - 80.0 °C |
174 - 1040 ksi @Temperature -40.0 - 176 °F |
Average value: 4.55 GPa Grade Count:1 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent, 0.5 in/min; ASTM D790 |
LyondellBasell Moplen EP/60 Bianco Polypropylene Copolymer Description: Moplen Coat EP/60 Bianco fractional melt flow, 1,200 MPa flexural modulus, extrusion grade polypropylene copolymer has a very good balance of properties and processability. Available in.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer Primary Processing Method: Injection Molding/ThermoformingKey Features: medium impact polypropylene copolymer resin for food packaging, FDA acceptable, low odor and low taste transfer, good cold imp.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 2541TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, HEAT STABILITY, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING SPECIALLY FOR WASHING TUB, ELECTRICAL APPLIANCES, THIN WALL CONTAINERS |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityAppli.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 75A6-2 Polypropylene Copolymer, 20% Calcium Carbonate Key Features: conventional melt flow, medium modulus, mineral-filled polypropylene copolymer, high impact, excellent chemical resistance, excellent aesthetics, high gloss, good colorability, good pr.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn SZ021-2 Polypropylene Copolymer, 20% Talc Key Features: medium melt flow, medium modulus, mineral-filled, utility grade polypropylene copolymer, good impact and stiffness balance, versatileApplications: inner door panels and seat supportsDe.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ CB251 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB251 medium melt flow, 1,200 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact resis.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ DR279 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ DR279 high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a unique balance of stiffness, impact resistance, processability.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM-D790 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPH 10099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 1099 is a controlled-rheology homopolymer having a very narrow molecular weight distribution. PPH 10099 is characterized by high fluidity for high speed spinning on spunla.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | cond; ISO 178 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant; ASTM D790 |
Braskem CP 204 Injection Molding Polypropylene Description: CP 204 is a high melt flow rate heterophasic copolymer with general purpose additive package. This product exhibits excellent processing performance, with good stiffness and impact stre.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C20L Calcium Reinforced |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ PB4432 TPO Compound Daplen PE4432 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen PE4432 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |