Material Notes:
Approx. H+ equivalent weight 65. Mix Ratio with GY 6010 is 35.Comments/Applications: Modified liquid amidoamine, low viscosity. Adhesives, coatings, flooring, potting and we lay-up applications. Bonds concrete. Cures in high humidity.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 500 - 900 cP
500 - 900 cP
Processing Properties Metric English Comments
Pot Life 30 min
30 min