Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.06 - 1.38 g/cc
0.0383 - 0.0499 lb/in³
Average value: 1.18 g/cc Grade Count:14
Filler Content 10.0 - 30.0 %
10.0 - 30.0 %
Average value: 21.3 % Grade Count:4
Water Absorption 0.0500 - 0.250 %
0.0500 - 0.250 %
Average value: 0.165 % Grade Count:11
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00517 cm/cm Grade Count:14
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 - 41.4 MPa
4000 - 6000 psi
Average value: 34.4 MPa Grade Count:11
Tensile Strength, Yield 3.45 - 34.5 MPa
500 - 5000 psi
Average value: 24.1 MPa Grade Count:3
Elongation at Break 1.80 - 10.0 %
1.80 - 10.0 %
Average value: 7.57 % Grade Count:11
Modulus of Elasticity 2.21 - 3.45 GPa
320 - 500 ksi
Average value: 2.81 GPa Grade Count:10
Flexural Yield Strength 27.6 - 68.9 MPa
4000 - 10000 psi
Average value: 52.5 MPa Grade Count:13
Flexural Modulus 2.41 - 3.20 GPa
350 - 464 ksi
Average value: 2.79 GPa Grade Count:14
Izod Impact, Notched 0.350 - 1.60 J/cm
0.656 - 3.00 ft-lb/in
Average value: 0.780 J/cm Grade Count:14
Izod Impact, Unnotched 2.67 - 8.01 J/cm
5.00 - 15.0 ft-lb/in
Average value: 4.50 J/cm Grade Count:7
Thermal Properties Metric English Comments
CTE, linear 41.4 µm/m-°C
23.0 µin/in-°F
Average value: 41.4 µm/m-°C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 93.3 - 102 °C
200 - 215 °F
Average value: 97.6 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 98.9 °C
176 - 210 °F
Average value: 90.3 °C Grade Count:8
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:11
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm
1.00e+15 - 1.00e+17 ohm-cm
Average value: 3.06e+16 ohm-cm Grade Count:7
Dielectric Strength 17.7 - 20.0 kV/mm
450 - 508 kV/in
Average value: 18.3 kV/mm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 199 - 232 °C
390 - 450 °F
Average value: 216 °C Grade Count:4
Melt Temperature 204 - 250 °C
400 - 482 °F
Average value: 227 °C Grade Count:7
Mold Temperature 50.0 - 85.0 °C
122 - 185 °F
Average value: 70.6 °C Grade Count:11
Drying Temperature 54.4 - 82.2 °C
130 - 180 °F
Average value: 73.7 °C Grade Count:7
Moisture Content 0.100 %
0.100 %
Average value: 0.100 % Grade Count:3
Dew Point -17.8 °C
0.000 °F
Average value: -17.8 °C Grade Count:3
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:7