Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-64 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer designed for glazing and sealing applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonat.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 8211-35W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 8211-45W237 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic general purpose non-hygroscopic elastomer, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processe.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
(discontinued **) Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-45W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-55 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | Optimum Tunnel temperature range. |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Processing Temperature | 180 - 232 °C | 356 - 450 °F | Average value: 205 °C Grade Count:6 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Processing Temperature | 199 - 232 °C | 390 - 450 °F | Average value: 216 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Processing Temperature | 215 - 232 °C | 419 - 450 °F | Preheat |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 188 - 232 °C | 370 - 450 °F | Blow Molding |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 192 - 232 °C | 378 - 450 °F | Stock temperature depending on base resin used |
Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate Characteristics: excellent thermal stability, a long useful outdoor life, good processabilityApplications: geomembranes, sheets and thermoforming, blow moldingProcessing: 192-232°C stock temperatur.. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Processing Temperature | 215 - 232 °C | 419 - 450 °F | Preheat |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Processing Temperature | 177 - 232 °C | 351 - 450 °F | |
ExxonMobil Vyram™ 9271-75 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |