Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.267 - 1.60 J/cm | 0.500 - 3.00 ft-lb/in | Average value: 0.570 J/cm Grade Count:31 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Izod Impact, Notched | 0.267 - 1.60 J/cm | 0.500 - 3.00 ft-lb/in | Average value: 0.625 J/cm Grade Count:107 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Notched | 0.588 - 1.60 J/cm | 1.10 - 3.00 ft-lb/in | Average value: 0.956 J/cm Grade Count:16 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.370 - 1.60 J/cm @Temperature -40.0 - 0.000 °C |
0.693 - 3.00 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.826 J/cm Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.350 - 1.60 J/cm | 0.656 - 3.00 ft-lb/in | Average value: 0.780 J/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 1.07 - 1.60 J/cm @Thickness 6.35 mm |
2.00 - 3.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.270 - 1.60 J/cm | 0.506 - 3.00 ft-lb/in | Average value: 0.813 J/cm Grade Count:19 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 1.07 - 1.60 J/cm @Temperature 23.0 °C |
2.00 - 3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® GND Acrylic/PVC Thermoplastic Sheet
(discontinued **) Conductive fire-rated sheetApplications: Electronic equipment where protection against electro-static damage is essential, conductive floor mats, IC containers like trays, storage bins, boxes, chip .. |
|||
Izod Impact, Notched | 0.587 - 1.60 J/cm | 1.10 - 3.00 ft-lb/in | Average value: 1.12 J/cm Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.700 - 1.60 J/cm | 1.31 - 3.00 ft-lb/in | Average value: 1.03 J/cm Grade Count:3 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 0.366 - 1.60 J/cm | 0.685 - 3.00 ft-lb/in | Average value: 0.940 J/cm Grade Count:14 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.908 - 1.60 J/cm | 1.70 - 3.00 ft-lb/in | Average value: 1.23 J/cm Grade Count:8 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched | 0.801 - 1.60 J/cm | 1.50 - 3.00 ft-lb/in | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Izod Impact, Notched | 1.07 - 1.60 J/cm | 2.00 - 3.00 ft-lb/in | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Izod Impact, Notched | 0.854 - 1.60 J/cm | 1.60 - 3.00 ft-lb/in | ASTM D256 |
Aaron Industries AVPS H 100-3 Virgin Polystyrene Melt flow index may be specified. |
|||
Izod Impact, Notched | 1.07 - 1.60 J/cm | 2.00 - 3.00 ft-lb/in | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Izod Impact, Notched | 0.534 - 1.60 J/cm | 1.00 - 3.00 ft-lb/in | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Izod Impact, Notched | 1.07 - 1.60 J/cm | 2.00 - 3.00 ft-lb/in | |
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti.. |
|||
Izod Impact, Notched | 0.530 - 1.60 J/cm | 0.993 - 3.00 ft-lb/in | Average value: 1.08 J/cm Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 0.534 - 1.60 J/cm | 1.00 - 3.00 ft-lb/in | Average value: 0.653 J/cm Grade Count:25 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Notched | 1.33 - 1.60 J/cm @Thickness 6.35 mm |
2.49 - 3.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-30GF/15T Modified PPO - 30% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.267 - 1.60 J/cm | 0.500 - 3.00 ft-lb/in | Average value: 0.534 J/cm Grade Count:35 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Izod Impact, Notched | 0.160 - 1.60 J/cm | 0.300 - 3.00 ft-lb/in | Average value: 0.404 J/cm Grade Count:21 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.587 - 1.60 J/cm | 1.10 - 3.00 ft-lb/in | Average value: 0.891 J/cm Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |