Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 98.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 98.9 °C
176 - 210 °F
Average value: 90.3 °C Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Deflection Temperature at 1.8 MPa (264 psi) 77.8 - 98.9 °C
172 - 210 °F
Average value: 90.6 °C Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 98.9 °C
170 - 210 °F
Average value: 87.7 °C Grade Count:14
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Deflection Temperature at 1.8 MPa (264 psi) 76.1 - 98.9 °C
169 - 210 °F
Average value: 91.9 °C Grade Count:4
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 98.9 °C
104 - 210 °F
Average value: 77.5 °C Grade Count:54
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..