Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | Average value: 34.4 MPa Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 26.5 - 41.4 MPa | 3840 - 6000 psi | Average value: 35.1 MPa Grade Count:4 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tensile Strength, Ultimate | 24.1 - 41.4 MPa | 3500 - 6000 psi | ASTM D638 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Tensile Strength, Ultimate | 34.5 - 41.4 MPa | 5000 - 6000 psi | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Tensile Strength, Ultimate | 27.6 - 41.4 MPa | 4000 - 6000 psi | ASTM D638 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer