Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 199 - 232 °C
390 - 450 °F
Average value: 216 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Processing Temperature 199 - 238 °C
390 - 460 °F
Average value: 220 °C Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Processing Temperature 199 - 213 °C
390 - 415 °F
Average value: 207 °C Grade Count:3
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Processing Temperature 199 - 249 °C
390 - 480 °F
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th..
Processing Temperature 199 - 216 °C
390 - 421 °F
Optimum Extrusion Temperature
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based  (discontinued **)
Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e..