Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Nylene® Norpex® AX245 PPE (Polyphenylene Ether)
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Nylene® Norpex® AX290 PPE (Polyphenylene Ether); High Performance High Heat
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Polykemi AB POLYfill PPC T8020 FC Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Density 1.06 g/cc
0.0383 lb/in³
Ineos ABS Centrex® 821 ASA Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection ..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Density 1.06 g/cc
0.0383 lb/in³
DIN 53479
Kraiburg TPE THERMOLAST® K TA8HAI Injection Molding TPE
Compound easy printable, paintable, glueable without pretreatmentColorable in any shadeSubstitution for PVC and silicone rubberTypical Applications: ToysBaby productsPromotion articlesMaterial Advan..
Density 1.06 g/cc
0.0383 lb/in³
Ineos ABS Lustran® PG 298
Key Features:UnfilledPlatableSuitable processing methods:Injection molding
Density 1.06 g/cc
0.0383 lb/in³
Momentive Performance Materials RTV1473 Black Adhesive Sealant, FIPG
One-part acetoxy cure. Typical uses: Heavy bodied adhesive sealant for formed-in-place gasketing. Good oil resistance.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..
Density 1.06 g/cc
0.0383 lb/in³
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding
Density 1.06 g/cc
0.0382 lb/in³
Fired Density at 2300°F
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44HS Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene
Features:Halogenated Forms:PelletsInformation provided by Multibase
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Lucobit Lucofin® 1413-t1 Polyolefin TPO Granules, Dark Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
LyondellBasell Hostacomâ„¢ XFBR712 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ XFBR712 medium melt flow, 1,800 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact resistance..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Techmer ES Elastoblend® PA6 IM HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific)
LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti..
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific)
Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. ..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Techmer ES Electrablend® HDPE C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackTPCI# 9411115Information provided by TP Composites, Inc.
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
SABIC Innovative Plastics Noryl EN130S PPE+HIPS (Europe-Africa-Middle East)
Noryl EN130S is an extrusion grade with a Vicat B/120 temperature of 140 deg C, developed for profile extrusion and in compliance with Food contact regulations; color limited.This data was supplied ..
Density 1.06 g/cc

@Temperature 50.0 °C
0.0383 lb/in³

@Temperature 122 °F
Solvay SOPROPHOR® TSP/724 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOPROPOXYLATED POLYARLYPHENOLCAS: 70880 – 56 – 7Solubility: Soluble in water and most polar and aromatic sol..
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Ensinger NORYL® Polyphenylene oxide (PPO)
NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Diamond Polymers NPP25-1202 TF20 20% Talc Filled Copolymer Polypropylene, Impact Modified, High Heat, High Stiffness with UV and Paintable Versions
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Aclo Accucomp ASA ASA001L
Density 1.06 g/cc
0.0383 lb/in³
3M 414DL Flexomount™ Solid Printing Tapes
3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system..
Density 1.06 g/cc
0.0383 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon P31000N010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: FEPSide 1: Uncured Silicone Rubber Substrate: PTFE Coated StockAppearance: Translucent silicone gum on release liners (clear and brown)This data represents typical v..
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
BASF Ultramid® HPN 9350 HS PA6 (Dry)
Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res..
Density 1.06 g/cc
0.0383 lb/in³
Uncured
3M Scotch-Weld™ EC2500 General Purpose Instant Adhesive
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me..
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Ashley Polymers Ashlene® 256 PPO
A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Lucobit Lucofin® 1412-t1 Polyolefin TPO Granules, Light Grey
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and ..