Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.21 - 2.90 GPa | 321 - 421 ksi | ASTM D638 |
Novatec Novacycle® 501 PVC Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe.. |
|||
Modulus of Elasticity | 2.21 - 3.45 GPa | 320 - 500 ksi | Average value: 2.81 GPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Modulus of Elasticity | 2.21 - 2.76 GPa | 320 - 400 ksi | Average value: 2.46 GPa Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 2.21 - 10.3 GPa | 321 - 1490 ksi | Average value: 4.47 GPa Grade Count:50 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Modulus of Elasticity | 2.21 - 7.50 GPa | 321 - 1090 ksi | Average value: 3.99 GPa Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Modulus of Elasticity | 2.21 - 11.7 GPa | 320 - 1700 ksi | Average value: 6.25 GPa Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 2.21 - 3.10 GPa | 320 - 450 ksi | Average value: 2.66 GPa Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |