Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.67 - 16.0 J/cm | 5.00 - 30.0 ft-lb/in | Average value: 5.32 J/cm Grade Count:64 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP (Asia Pacific) LNP* Thermocomp* MFB429 is a compound based on Polypropylene resin containing Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.67 - 4.27 J/cm | 5.00 - 8.00 ft-lb/in | Average value: 3.42 J/cm Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Izod Impact, Unnotched | 2.67 - 8.54 J/cm | 5.00 - 16.0 ft-lb/in | Average value: 5.49 J/cm Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched | 2.67 - 5.34 J/cm | 5.00 - 10.0 ft-lb/in | Average value: 3.63 J/cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |