Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ G1550S High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC PP 524P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 524P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC PP 529P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 529P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Izod Impact, Notched | >= 0.350 J/cm @Temperature 23.0 °C |
>= 0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 4215M (EP1X35F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.350 - 1.60 J/cm | 0.656 - 3.00 ft-lb/in | Average value: 0.780 J/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler
(discontinued **) Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa.. |
|||
Izod Impact, Notched | 0.350 - 0.480 J/cm @Temperature -40.0 - -40.0 °C |
0.656 - 0.899 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.427 J/cm Grade Count:5 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem HC 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East) 10% GF FR PBT/PC Blend |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM-D256 |
Braskem H 503HS HOMO Polypropylene Homopolymer H 503HS is a low melt flow rate homopolymer for general purpose. It is designed for raffia extrusion and fiber extrusion. This product exhibits excellent processability, high speed production with g.. |
|||
Izod Impact, Notched | 0.350 - 1.08 J/cm | 0.656 - 2.02 ft-lb/in | Average value: 0.713 J/cm Grade Count:32 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |