Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 80.0 - 82.2 °C | 176 - 180 °F | Average value: 81.8 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |