Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+6 - 1.00e+17 ohm-cm | 1.00e+6 - 1.00e+17 ohm-cm | Average value: 9.89e+15 ohm-cm Grade Count:55 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Electrical Resistivity | 1.00e+16 - 1.00e+17 ohm-cm | 1.00e+16 - 1.00e+17 ohm-cm | Average value: 1.89e+16 ohm-cm Grade Count:43 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | 4000 - 1.00e+17 ohm-cm | 4000 - 1.00e+17 ohm-cm | Average value: 6.60e+15 ohm-cm Grade Count:17 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+17 ohm-cm | 1.00e+14 - 1.00e+17 ohm-cm | Average value: 2.55e+16 ohm-cm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+17 ohm-cm | 1.00e+15 - 1.00e+17 ohm-cm | Average value: 1.29e+16 ohm-cm Grade Count:29 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+17 ohm-cm | 1.00e+13 - 1.00e+17 ohm-cm | Average value: 4.52e+16 ohm-cm Grade Count:12 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+17 ohm-cm | 1.00e+13 - 1.00e+17 ohm-cm | Average value: 1.18e+16 ohm-cm Grade Count:64 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Electrical Resistivity | 1.00e+10 - 1.00e+17 ohm-cm | 1.00e+10 - 1.00e+17 ohm-cm | Average value: 3.49e+15 ohm-cm Grade Count:36 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Electrical Resistivity | 100 - 1.00e+17 ohm-cm | 100 - 1.00e+17 ohm-cm | Average value: 5.11e+15 ohm-cm Grade Count:37 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Electrical Resistivity | 100 - 1.00e+17 ohm-cm | 100 - 1.00e+17 ohm-cm | Average value: 5.00e+16 ohm-cm Grade Count:9 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+17 ohm-cm | 1.00e+15 - 1.00e+17 ohm-cm | Average value: 4.71e+16 ohm-cm Grade Count:18 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+17 ohm-cm | 1.00e+14 - 1.00e+17 ohm-cm | Average value: 1.70e+16 ohm-cm Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+17 ohm-cm | 1.00e+12 - 1.00e+17 ohm-cm | Average value: 5.95e+15 ohm-cm Grade Count:52 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+17 ohm-cm | 1.00e+15 - 1.00e+17 ohm-cm | Average value: 2.57e+16 ohm-cm Grade Count:4 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+17 ohm-cm | 1.00e+12 - 1.00e+17 ohm-cm | Average value: 3.65e+15 ohm-cm Grade Count:61 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 7.97e+15 ohm-cm Grade Count:40 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm | 1.00e+9 - 1.00e+17 ohm-cm | Average value: 2.75e+15 ohm-cm Grade Count:44 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+17 ohm-cm | 1.00e+15 - 1.00e+17 ohm-cm | Average value: 5.05e+16 ohm-cm Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Electrical Resistivity | 1.00e+16 - 1.00e+17 ohm-cm | 1.00e+16 - 1.00e+17 ohm-cm | Average value: 2.80e+16 ohm-cm Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+17 ohm-cm | 1.00e+8 - 1.00e+17 ohm-cm | Average value: 1.90e+15 ohm-cm Grade Count:64 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Electrical Resistivity | 6.60 - 1.00e+17 ohm-cm | 6.60 - 1.00e+17 ohm-cm | Average value: 9.88e+15 ohm-cm Grade Count:124 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Electrical Resistivity | 200 - 1.00e+17 ohm-cm | 200 - 1.00e+17 ohm-cm | Average value: 1.01e+16 ohm-cm Grade Count:22 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.58e+15 ohm-cm Grade Count:28 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+17 ohm-cm | 1.00e+15 - 1.00e+17 ohm-cm | Average value: 2.74e+16 ohm-cm Grade Count:14 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Electrical Resistivity | 10.0 - 1.00e+17 ohm-cm | 10.0 - 1.00e+17 ohm-cm | Average value: 4.60e+15 ohm-cm Grade Count:80 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+17 ohm-cm | 1.00e+14 - 1.00e+17 ohm-cm | Average value: 1.69e+16 ohm-cm Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Electrical Resistivity | 1.00 - 1.00e+17 ohm-cm | 1.00 - 1.00e+17 ohm-cm | Average value: 2.63e+15 ohm-cm Grade Count:46 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 1.16e+16 ohm-cm Grade Count:54 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 5.41e+15 ohm-cm Grade Count:48 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 8.62e+15 ohm-cm Grade Count:26 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |