Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.Applications: MedicalTechnical Data Sheet General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.Information provided by Eastman Chemical.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792 and ISO 1183D
Water Absorption 0.13 %
0.13 %
24 hour immersion; ISO 62
Moisture Vapor Transmission 6.00 cc-mm/m²-24hr-atm
15.2 cc-mil/100 in²-24hr-atm
F 372 Test conducted at 38°C (100°F) and 100% relative humidity.
Oxygen Transmission 10.0 cc-mm/m²-24hr-atm
25.4 cc-mil/100 in²-24hr-atm
ASTM D3985
Viscosity Measurement 0.70
0.70
0.7 for films per EMN-A-AC-G-V-1
0.70
0.70
inherent viscosity of pellets
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ISO 2039-2
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ISO 527
Film Tensile Strength at Yield, MD 52.0 MPa
7540 psi
ASTM D882
Film Tensile Strength at Yield, TD 52.0 MPa
7540 psi
ASTM D882
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 400 %
400 %
ASTM D882
Film Elongation at Yield, MD 4.0 %
4.0 %
ASTM D882
Film Elongation at Yield, TD 4.0 %
4.0 %
ASTM D882
Elongation at Break 100 %
100 %
ISO 527
Tensile Modulus 2.10 GPa
305 ksi
ISO 527
Flexural Yield Strength 68.0 MPa
9860 psi
ISO 178
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Secant Modulus, MD 1.90 GPa
276 ksi
ASTM D882
Secant Modulus, TD 1.90 GPa
276 ksi
ASTM D882
Izod Impact, Notched 1.01 J/cm
1.89 ft-lb/in
ASTM D256
0.370 J/cm

@Temperature -40.0 °C
0.693 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Elmendorf Tear Strength, MD 13.7 g/micron
348 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 16.7 g/micron
424 g/mil
ASTM D1922
Dart Drop Test 400 g
0.882 lb
Modified 12.7 mm (0.5 in.) dia. head, 127 mm (5 in.) dia. clamp, 660 mm (26 in.) drop. Value at -18°C (0°F) is 500 g.; ASTM D1709A
Film Tensile Strength at Break, MD 59.0 MPa
8560 psi
ASTM D882
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C

@Temperature -30.0 - 40.0 °C
28.3 µin/in-°F

@Temperature -22.0 - 104 °F
ASTM D696
Specific Heat Capacity 1.30 J/g-°C

@Temperature 60.0 °C
0.311 BTU/lb-°F

@Temperature 140 °F
1.76 J/g-°C

@Temperature 100 °C
0.421 BTU/lb-°F

@Temperature 212 °F
1.88 J/g-°C

@Temperature 150 °C
0.449 BTU/lb-°F

@Temperature 302 °F
1.97 J/g-°C

@Temperature 200 °C
0.471 BTU/lb-°F

@Temperature 392 °F
2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Glass Transition Temp, Tg 80.0 °C
176 °F
DSC
Optical Properties Metric English Comments
Haze 0.80 %
0.80 %
ASTM D1003
Gloss 108 %
108 %
at 45°; ASTM D 2457
Transmission, Visible 85 %
85 %
per ASTM D1746
89 %
89 %
Regular transmittance per ASTM D 1003 Modified.
91 %
91 %
Total Transmittance; ASTM D 1003
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 2.4

@Frequency 1e+6 Hz
2.4

@Frequency 1e+6 Hz
ASTM D 150
2.6

@Frequency 1000 Hz
2.6

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
Short Time, 500 V/sec rate-of-rise; ASTM D 149
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz
ASTM D150
0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 143 sec
143 sec
ASTM D495