Material Notes:
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combination with low fume toxicity (RATP* approved), outstanding processability - optimized for automatic processing.This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS)Processing: Injection and transfer molding. Applications: Thermostat housings, Switch parts and RelaysInformation provided by the Raschig Group
Physical Properties Metric English Comments
Specific Gravity 1.90 - 2.10 g/cc
1.90 - 2.10 g/cc
ISO 1183
Apparent Bulk Density 0.700 - 0.850 g/cc
0.0253 - 0.0307 lb/in³
ISO 60
Water Absorption <= 0.30 %

@Temperature 23.0 °C,
Time 86400 sec
<= 0.30 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0020 - 0.0045 cm/cm
0.0020 - 0.0045 in/in
Injection; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 - 70.0 MPa
8700 - 10200 psi
Injection; ISO 527
Modulus of Elasticity 13.0 - 15.0 GPa
1890 - 2180 ksi
Injection; ISO 527
Flexural Strength 140 - 160 MPa
20300 - 23200 psi
Injection; ISO 178
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Injection; ISO 178
Compressive Strength 100 - 150 MPa
14500 - 21800 psi
Injection; ISO 604
Charpy Impact Unnotched 1.40 - 1.60 J/cm²

@Temperature 23.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Charpy Impact, Notched 0.500 - 0.600 J/cm²

@Temperature 23.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Thermal Properties Metric English Comments
CTE, linear 10.0 - 20.0 µm/m-°C

@Temperature 50.0 - 100 °C
5.56 - 11.1 µin/in-°F

@Temperature 122 - 212 °F
Injection; ISO 11359-2
Thermal Conductivity 0.900 - 1.10 W/m-K
6.25 - 7.63 BTU-in/hr-ft²-°F
ASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
Injection; ISO 75-A
Deflection Temperature at 8.0 MPa 130 - 150 °C
266 - 302 °F
Injection; ISO 75-C
Flammability, UL94 V-0

@Thickness 1.10 mm
V-0

@Thickness 0.0433 in
Shrinkage <= 0.050 %

@Temperature 110 °C,
Time 605000 sec
<= 0.050 %

@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cm
1.00e+14 - 1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 - 1.00e+14 ohm
1.00e+13 - 1.00e+14 ohm
IEC 60093
Dielectric Constant 4.0 - 5.0

@Frequency 1.00e+6 Hz
4.0 - 5.0

@Frequency 1.00e+6 Hz
IEC 60250
5.0 - 6.0

@Frequency 100 Hz
5.0 - 6.0

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 - 35.0 kV/mm
635 - 889 kV/in
IEC 60243-1
Dissipation Factor 0.010 - 0.030

@Frequency 100 Hz
0.010 - 0.030

@Frequency 100 Hz
IEC 60250
0.010 - 0.030

@Frequency 1.00e+6 Hz
0.010 - 0.030

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
CTI; IEC 60112
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 15.0 - 25.0 °C
6.00 Month

@Temperature 59.0 - 77.0 °F
Descriptive Properties Value Comments
Arc Resistance 4 Stufe
ASTM D495
Glow wire flammability test 960/1
IEC 60695 2-12
Glow wire ignitability test 930/1
IEC 60695 2-13
Water Absorption <20 mg
ISO 62; 24h / 23°C