Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ASTM D882 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ASTM D882 |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ISO 527-3 |
Borealis FS1560 High Density Polyethylene FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ISO 527-3 |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ISO 527-3 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ISO 527-3 |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ASTM D882 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ASTM D882 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Film Tensile Strength at Break, TD | 55.0 MPa | 7980 psi | ISO 527-3 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |