Polymer Property : Elmendorf Tear Strength, TD = 424 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 16.7 g/micron
424 g/mil
ASTM D1922
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..