Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5005 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5005 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typical applications include merchandise bags, grocery sacks, trash can liners, produce bags and roll stock.Regulatory StatusL 5005 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing L 5005 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Process Condition Ranges: BUR=3.5-4.5:1; Neck Height=6-9 Die Diameters: Die Gap(nominal), in.=0.040-0.050; Tower Height=Relatively Short; Output, Lb/Hr/In of Die Circumference=10-12; Melt Temperature- 390-420°F(199-216°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Melt Flow 0.057 g/10 min
0.057 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D882
Film Tensile Strength at Yield, TD 23.4 MPa
3400 psi
ASTM D882
Film Elongation at Break, MD 300 %
300 %
ASTM D882
Film Elongation at Break, TD 420 %
420 %
ASTM D882
Elmendorf Tear Strength MD 14 g
14 g
ASTM D1922
Elmendorf Tear Strength TD 35 g
35 g
ASTM D1922
Dart Drop Total Energy 1090 J/cm
2.05 ft-lb/mil
ASTM D3420
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Film Tensile Strength at Break, TD 34.5 MPa
5000 psi
ASTM D882
1% Secant Modulus, MD 793 MPa
115000 psi
ASTM D822
1% Secant Modulus, TD 965 MPa
140000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 - 216 °C
390 - 421 °F