Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.88 J/g-°C @Temperature 150 °C |
0.449 BTU/lb-°F @Temperature 302 °F |
|
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Specific Heat Capacity | 1.88 J/g-°C @Temperature 157 °C |
0.449 BTU/lb-°F @Temperature 315 °F |
solid |
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |
|||
Specific Heat Capacity | 1.88 J/g-°C @Temperature 150 °C |
0.449 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Specific Heat Capacity | 1.88 J/g-°C @Temperature 150 °C |
0.449 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |