Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.0 - 19.0 kV/mm @Thickness 0.100 mm |
406 - 483 kV/in @Thickness 0.00394 in |
short term; ASTM D149 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | ASTM D149 |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | D149 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Dielectric Strength | >= 16.0 kV/mm @Thickness 3.17 mm |
>= 406 kV/in @Thickness 0.125 in |
ASTM D149 |
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Dielectric Strength | >= 16.0 kV/mm @Thickness 3.17 mm |
>= 406 kV/in @Thickness 0.125 in |
ASTM D149 |
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
Cookson Group Plaskon® 1002 Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Dielectric Strength | >= 16.0 kV/mm | >= 406 kV/in | |
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | Perpendicular (ASTM D149), Short Time |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | GB/T1408.1-2006 |
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL ENV150 PPE (Europe-Africa-Middle East) Noryl* ENV150 modified polyphenylene ether resin is an unfilled, flame retardant high heat grade suitable for extrusion molding conversion route. It uses non-chlorinated, non-brominated FR additives.. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | IEC 60243 |
Solvay TECHNYL® 2710IR PA66, Conditioned Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
3M Scotchkote™ 80FG 532 Urethane Elastomer Scotchkote Urethane Elastomer 80FG 532 has been specifically developed as an elastomeric system with a high degree of flexibility for casting and molding rubber components.Product Features:Propertie.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | |
3M Scotchkote™ 75RG 530 Urethane Elastomer Scotchkote Urethane Elastomer 75RG 530 has been specifically developed as a fast curing 75-80 Durometer, elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing r.. |
|||
Dielectric Strength | 16.0 - 90.0 kV/mm | 406 - 2290 kV/in | Average value: 40.0 kV/mm Grade Count:9 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Dielectric Strength | 16.0 kV/mm | 406 kV/in | 60Hz, Short Time, wet; ASTM D149 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |